EASA Certification Specifications with AMCFinal — current published edition checked

CS-25

Large Aeroplanes

Amendment 28; corrected 20 November 2025 Source checked 2026-11-28

Scope, source and reading notes

Complete official CS-25 Amendment 28, including AMC and appendices.

Aerospace Consulting reference note: Certification specifications and acceptable means of compliance for large aeroplanes, using the corrected official publication.

The complete selected publication is available in reading text and as the original PDF. Reading text is extracted from the official PDF; page layout is simplified, and figures and tables should be checked in the original page view.

Search covers extracted text. Words contained only in graphics may not be searchable. The original publication is available below.

Official source recordOriginal PDF on this site

Source: EASA. Reproduced with source acknowledgment; source edition and status are shown above. SHA-256: 32f1a9acf26e8ceceb291d206bf07a7071f7f59f40f10c096bb17f34c6a58007

Source page 1300 · PDF page 1300

exposed surface of the specimen, which passes through its vertical centreline and must be pointed toward the radiation source. The gas supplied to the burner must be methane adjusted to produce flame lengths of 25 mm.

(c) Calibration of Equipment

(1) Heat Release Rate. A burner as shown in Figure 4 must be placed over the end of the lower pilot flame tubing using a gas-tight connection. The flow of gas to the pilot flame must be at least 99% methane and must be accurately metered. Prior to usage, the wet test meter is properly levelled and filled with distilled water to the tip of the internal pointer while no gas is flowing. Ambient temperature and pressure of the water, are based on the internal wet test meter temperature. A baseline flow rate of approximately 1 litre/min. is set and increased to higher preset flows of 4, 6, 8, 6 and 4 litres/min. The rate is determined by using a stopwatch to time a complete revolution of the west test meter for both the baseline and higher flow, with the flow returned to baseline before changing to the next higher flow. The thermopile baseline voltage is measured. The gas flow to the burner must be increased to the higher preset flow and allowed to burn for 2·0 minutes, and the thermopile voltage must be measured. The sequence is repeated until all five values have been determined. The average of the five values must be used as the calibration factor. The procedure must be repeated if the percent relative standard deviation is greater than 5%. Calculations are shown in paragraph (f).

(2) Flux Uniformity. Uniformity of flux over the specimen must be checked periodically and after each heating element change to determine if it is within acceptable limits of ± 5%.

(d) Sample Preparation

(1) The standard size for vertically mounted specimens is 150 x 150 mm with thicknesses up to 45 mm.

(2) Conditioning. Specimens must be conditioned as described in Part 1 of this Appendix.

(3) Mounting. Only one surface of a specimen will be exposed during a test. A single layer of 0·025 mm aluminium foil is wrapped tightly on all unexposed sides.

(e) Procedure

(1) The power supply to the radiant panel is set to produce a radiant flux of 3·5 Watts/cm2. The flux is measured at the point, which the centre of the specimen surface will occupy when positioned for test. The radiant flux is measured after the airflow through the equipment is adjusted to the desired rate. The sample should be tested in its end use thickness.

(2) The pilot flames are lighted and their position, as described in sub-paragraph (b)(8), is checked.

(3) The airflow to the equipment is set at 0·04 ± 0·001 m3/s at atmospheric pressure. Proper air flow may be set and monitored by either: (1) An orifice meter designed to produce a pressure drop of at least 200 mm of the manometric fluid, or by (2) a rotometer (variable orifice meter) with a scale capable of being read to ± 0·0004 m3/s. The stop on the vertical specimen holder rod is adjusted so that the exposed surface of the specimen is positioned 100 mm from the entrance when injected into the environmental chamber.

(4) The specimen is placed in the hold chamber with the radiation doors closed. The airtight outer door is secured, and the recording devices are started. The specimen must be retained in the hold chamber for 60 seconds ± 10 seconds, before injection. The thermopile “zero” value is determined during the last 20 seconds of the hold period.

Connected references

Source-backed citations and subject-based engineering context are labelled separately. These links do not establish equivalence or project acceptance.

AMC 20-152A

Listed as related material by

Source-backed
Evidence and scope

AMC 20-152A §8(a)(2)

Lists CS-25 without an amendment or specific paragraph.

Family reference; does not select a certification basis.

Supporting source

Copy reference

Select and copy the citation below.