AC 27-1B, Chg 4 12/1/2011
(A) Damage Tolerant Safe-Life Evaluation. This is a “No-Growth” method in
which the structure, with damage present, is able to withstand repeated loads of
variable magnitude without detectable damage growth for the life of the rotorcraft or
within a specified replacement time. This evaluation may be used to substantiate any
type of damage that will remain in-service for the life of the part.
No specific inspection requirements are generated from the test program in this method.
However, compliance with routine inspections for cracking, delaminations, and service
damage and other limitations prescribed in accordance with § 27.1529 are always
required. Compliance using full-scale, component, or sub-component fatigue testing
can be accomplished by either of the following methods:
(1) S-N Method. This method is based on determining the point where
initiation of growth occurs for the damage present at critical locations in the structure.
AC 27-1B, AC 27 MG 11, provides guidance that may be appropriate for this method.
The method utilizes one or more full-scale, component, or sub-component test
specimens subjected to constant-amplitude or spectrum loading applied in a distribution
on the structure that is representative of critical flight conditions. Any indication of
growth of the imposed damage and defects, or structurally significant cracking,
disbonding, splintering, or delaminating of the composite, defines the fatigue initiation
characteristic of the structure in terms of applied load and cycles. Working S-N curves
are established from the mean curve using strength or cycle reductions or both to
account for fatigue scatter and environmental effects. Flight loads are compared to this
working curve, and if any intercepts occur, a cumulative damage calculation is
conducted to establish the component retirement time. Compliance with the ultimate
load requirements should be demonstrated at the completion of the fatigue test.
(2) Life-Test Method. This method uses spectrum fatigue testing to verify the
absence of damage growth over a large number of cycles that are equivalent to a
lifetime of expected usage. The method uses one or more full-scale, component, or
sub-component test specimens subjected to spectrum fatigue loading applied in a
representative distribution of flight loads, including Ground-Air-Ground (GAG) loads.
Fatigue test loads should be increased by factors for environment and fatigue strength
scatter. The load may also be increased using an S-N curve approach to reduce the
duration of the test. Any significant growth of the imposed damage, or structurally
significant cracking, disbonding, splintering, or delamination of the composite during the
test constitutes failure to achieve the desired lifetime. However, the equivalent life
demonstrated at the time of inception of damage growth or cracking can be used as a
retirement time for the component. Compliance with the ultimate load requirements
should be demonstrated at the completion of the fatigue test.
(B) Damage Tolerant Fail-Safe (Residual Strength with Detectable Damage)
Evaluation. This method establishes inspection intervals to ensure that the structure
remaining after a partial failure is able to withstand design limit loads without failure or
excessive structural deformations within a specified inspection interval. If the damage is
detected in an inspection, the structure should be either replaced or repaired to restore
Page C - 110